摘要:

以单侧双排四通管液压胀形工艺为研究对象,运用数值模拟方法分析不同加载参数条件下单侧双排四通管液压胀形支管高度、壁厚分布和补料情况,得出单侧双排四通管液压胀形壁厚分布和补料的一般规律。结果表明:单侧双排四通管液压胀形以两支管外侧主管补料为主,支管间内侧主管补料很少。加载参数对支管高度和外侧主管补料影响较大,对最大、最小壁厚值和内侧主管补料影响很小。内侧主管壁厚分布比较均匀,厚度分界线在外侧主管且靠近支管区域。

Unilateral double four-way tube hydroforming technology was considered as the research object, numerical simulation method was utilized to analyze branch height, thickness distribution and feeding for unilateral double four-way tube hydroforming under different loading paths, then ,general rule of distribution and feeding for unilateral double four-way tube hydroforming was obtained.Results suggest that feeding of unilateral double four-way tube hydroforming relies mainly on tube outside two branches, feeding of inside tube between two branches is little. Loading path influences much on branches height and outside tube feeding, it influences little on maximum and minimum thickness and inside tube feeding. The inside tube thickness distribution is homogeneous, and thickness dividing line is on outside tube and closes to branch.

基金项目:
国家自然科学基金资助项目(U0934006)
作者简介:
参考文献:

[1]苑世剑.现代液压成形技术[M].北京:国防工业出版社,2009.

[2]王宗堂,张士宏,梁海成,等.三通管内高压成形工艺研究[J].锻压技术,2008,33(2):63-65.

[3]Hartl Ch. Research and advances in fundamentals and industrial applications of hydroforming[J]. J.Mates.Proc.Tech.,2005,167: 383-392.

[4]Nishant Jain, Jyhwen Wang, Richard Alexander. Finite element analysis of dual hydroforming process[J].J.Mates.Proc.Tech.,2004,145:59-65.

[5]Giuseppe Ingarao, Rosa Di Lorenzo, fabrizio Micari.Internal pressure and counterpunch action design in Y-shaped tube hydroforming process:Amulti\|objective optimisation approach[J].J.Mates.Proc.Tech.,2009,87: 591-602.

[6]苑世剑.变径管内高压成形送料区壁厚分布规律[J].塑性工程学报, 2008,15(4):37-40.

[7]苑文婧,王小松,苑世剑.变径管内高压成形厚度分界圆[J].材料科学与工艺,2008,16(2):196-199.

[8]袁安营, 张士宏,王忠堂,等.管材内高压成形新加载方式的研究[J].锻压技术,2008,33(5):95-98.

[9]程东明,滕步刚,郭斌,等.Y型三通管内高压成形壁厚分布规律[J] .材料科学与工艺,2007,15(6):750-753.

[10]翟江波.多通管液压胀形工艺仿真及成形控制模式研究[D] .西安:西北工业大学,2007.

服务与反馈:
本网站尚未开通全文下载服务】【加入收藏
《锻压技术》编辑部版权所有

中国机械工业联合会主管  中国机械总院集团北京机电研究所有限公司 中国机械工程学会主办
联系地址:北京市海淀区学清路18号 邮编:100083
电话:+86-010-82415085 传真:+86-010-62920652
E-mail: fst@263.net(稿件) dyjsjournal@163.com(广告)
京ICP备07007000号-9