[1]何文治.航空制造工程手册[M].北京:航空工业出版社,1992.
He W Z. Aviation Manufacturing Engineering Handbook[M]. Beijing: Aviation Industry Press, 1992.
[2]程鹏志.导管数控弯曲成形质量预测与工艺优化技术研究[D].北京:北京理工大学,2010.
Cheng P Z. Research on Quality Forecast and Parameters Optimization Technology of NC Tube Bending[D]. Beijing: Beijing Institute of Technology, 2010.
[3]Gao L, Mostch S, Strano M,Classification and analysis of tube hydroforming processes with respect to adaptive FEM simulations[J]. Journal of Materials Processing Technology, 2002,37(5): 22-26.
[4]Prabhu A, Mishra N, Narasimhan N. A study on the effect of pre-bending radius on the formability of hydroformed steel tubes[A]. The 8th International Conference and Workshop on Numerical Simulation of 3D Sheet Metal Forming Processes[C]. Seoul, 2011.
[5]岳永保,杨合,詹梅,等.薄壁管小弯曲半径数控弯曲壁厚减薄实验研究[J].锻压技术,2007,32(5):58-62.
Yue Y B, Yang H, Zhan M, et al. Experimental study on thinning of thin-walled tube NC bending process with small bending radius[J]. Forging & Stamping Technology, 2007, 32(5): 58-62.
[6]李恒,杨合,詹梅,等.大口径薄壁小弯曲半径数控弯管有限元建模和实验[J].锻压技术,2006,31(5):136-139.
Li H, Yang H, Zhan M, et al. FEM modeling and experimental of NC bending process of thin-wall tube with large diameter and small bending radius[J]. Forging & Stamping Technology, 2006, 31(5): 136-139.
[7]鄂大辛,宁汝新,唐承统,等.壁厚变形对弯管最小相对弯曲半径的影响[J].锻压技术,2006,31(1):90-93.
E D X, Ning R X, Tang C T, et al. Influence of wall thickness deformation upon the minimum bending radius of bending tube[J]. Forging & Stamping Technology, 2006, 31(1): 90-93.
[8]苑世剑,刘刚,何祝斌,等.内高压成形机理与关键技术[J].数字制造科学,2008,6(4):1-34.
Yuan S J, Liu G, He Z B, et al. Mechanism of internal high pressure forming and its key technologies[J]. Digital Manufacture Science, 2008, 6(4): 1-34.
[9]苑世剑.现代液压成形技术[M].北京:国防工业出版社,2009.
Yuan S J. Modern Hydroforming Technology[M]. Beijing: National Defence Industry Press, 2009.
|