摘要:
为了深入研究4032铝合金活塞在热模锻过程中的材料变形特性,建立了典型活塞热模锻工艺的热-塑耦合有限元模型,详细研究了坯料的不同变形区域在锻造过程中的温度场变化、材料流动规律和应力、应变状态,进而分析了活塞锻件的预期力学性能和潜在锻造缺陷产生机理。模拟获得了锻造力曲线和锻件外形尺寸,通过对比模拟结果与实际锻件的关键几何参数,验证了有限元模型的合理性。模拟结果指出:材料变形由上模的冲孔和反挤压运动产生,材料变形区集中于上模冲孔面和台阶面附近,坯料在锻造过程中整体处于三向压应力状态;活塞内表面微小折叠、划伤、材料剥离等锻造缺陷和活塞裙填充不足、高度不均匀等工艺问题,主要是由模具的摩擦作用和材料流向的突变导致,实际生产过程应严格控制上模的表面精度和润滑效果,并应注意模具轴向棱边的圆滑设计。
In order to study the deformation characteristics of 4032 aluminum alloy piston during the hot die forging process deeply, a thermo-plastic coupled finite element model of hot die forging process for a typical piston was established, and the temperature field, the flow law of materials and the strain-stress state at the different deformation areas of blank during the forging process were studied in detail. Then, the expected mechanical performance and the mechanism of potential forging defects for the forged pistons were analyzed. Furthermore, the forging force curve and the overall dimension of the forged pistons were obtained, and the rationality of the finite element model was verified by comparing the simulation results with the key geometric parameters of the actual forged pistons. The simulation results show that the material deformation of piston is caused by piercing and backward extruding of upper die, the material deformation mainly occurs in the areas near the piercing and stepped surfaces of upper die, and the blank is in a three-way compressive stress state during the forging process. In addition, the forging defects such as micro-folding, scratching, material peeling on the inner surface of piston and the process problems such as insufficient filling and height unevenness of piston skirt are mainly caused by the friction of die and the sudden change of material flow directions. Thus, the surface precision and the lubrication effect of upper die should be strictly controlled, and the smooth design on the axial edges of die should be paid attention in the actual production process.
基金项目:
国家重点研发计划“智能农机装备”重点专项(2017YFD0700200);中国博士后科学基金(2018M643627)
作者简介:
张超(1989-),男,博士研究生,E-mail:zhangc_xjtu@qq.com;通讯作者:赵升吨(1962-),男,博士,教授,E-mail:sdzhao@xjtu.edu.cn
参考文献:
[1]陈长江,王渠东,尹冬弟,等.内燃机活塞材料的研究进展[J].材料导报,2009,23(15):62-65.
Chen C J, Wang Q D,Yin D D, et al. Research process in piston materials of combustion engine [J]. Materials Reports, 2009, 23(15): 62-65.
[2]王玉凤.4032铝合金组织及力学性能分析[D].哈尔滨:哈尔滨工业大学,2010.
Wang Y F. Study of the Microstructures and Mechanical Properties of 4032 Alloy[D]. Harbin: Harbin Institute of Technology, 2010.
[3]Hong J T, Lee S R, Park C H, et al. Iterative preform design technique by tracing the material flow along the deformation path: Application to piston forging [J]. Engineering Computations: International Journal for Computer-aided Engineering and Software, 2006, 23(1): 16-31.
[4]史瑱.4032铝合金高温变形行为及涡旋盘精密模锻数值模拟[D].哈尔滨:哈尔滨工业大学,2010.
Shi S. High Temperature Deformation Behavior and Numerical Simulation on Precision Die Forging for Scroll of 4032 Aluminum Alloy [D]. Harbin: Harbin Institute of Technology, 2010.
[5]陈满,王匀,许桢英,等.4032 铝合金花盘锻压成形技术[J].锻压技术,2017,42(7):13-18.
Chen M, Wang Y, Xu Z Y, et al. Forging technology of aluminum alloy 4032 faceplate [J]. Forging & Stamping Technology, 2017, 42(7): 13-18.
[6]周飞,彭颖红,雷军,等.LD11铝合金活塞裙锻造成形坯料工艺[J].上海交通大学学报,2001,35(1):86-89.
Zhou F, Peng Y H, Lei J, et al. Billets study during piston skirt forging process of LD11 aluminum alloy [J]. Journal of Shanghai Jiaotong University, 2001, 35(1): 86-89.
[7]Dong W P, Chen J. 3D FEA simulation of 4A11 piston skirt isothermal forging process [J]. Transactions of Nonferrous Metals Society of China, 2008, 18(5): 1196-1200.
[8]孙绍华,左宏卿,孙超.铝合金V26-1活塞模锻件精化设计与锻压工艺改进[J].轻合金加工技术,2010,38(9):32-36.
Sun S H, Zuo H Q, Sun C. Precision design and improvement of forging technology of V26-1 aluminum alloy piston [J]. Light Alloy Fabrication Technology, 2010, 38(9): 32-36.
[9]马晓琴,张育国,张镭,等.变形铝合金活塞成形工艺数值分析[J].热加工工艺,2012,41(23):104-106.
Ma X Q, Zhang Y G, Zhang L, et al. Numerical analysis on forming process of wrought aluminum alloy piston [J]. Hot Working Technology, 2012, 41(23): 104-106.
[10]肖爱武.铝合金活塞模锻件的锻压工艺优化[J].轻合金加工技术,2017,45(1):35-39.
Xiao A W. Forging process optimization of aluminum alloy piston die forging [J]. Light Alloy Fabrication Technology, 2017, 45(1): 35-39.
[11]邵镇海.4032铝合金塑性变形的应用基础研究[D].武汉:华中科技大学,2009.
Shao Z H. Basic Study on Applying the Plastic Forming of 4032 Al-Alloy [D]. Wuhan: Huazhong University of Science & Technology, 2009.
[12]陈艳.高性能活塞用4032B挤压铝合金的研制[D].长沙:中南大学,2010.
Chen Y. Development of 4032B Extruded Aluminum Alloy for Piston of High Performance [D]. Changsha: Central South University, 2010.
[13]万帆,运新兵,毕胜,等.成形工艺对铝锶合金组织性能及细化性能的影响[J].稀有金属,2018,42(8):799-806.
Wan F, Yun X B, Bi S,et al. Microstructure, properties and refining performance of Al-Si alloy under different forming process [J]. Chinese Journal of Rare Metals, 2018, 42(8): 799-806.
[14]徐祥,杨明,梁益龙,等.211Z.X耐热高强韧铝合金的热变形行为研究[J].稀有金属,2017,41(9):964-971.
Xu X, Yang M, Liang Y L, et al. Hot deformation and constitutive model by strain compensation of 211Z.X heat-resisting high strength and toughness aluminum alloy [J]. Chinese Journal of Rare Metals, 2017, 41(9): 964-971.
服务与反馈:
本网站尚未开通全文下载服务】【加入收藏
《锻压技术》编辑部版权所有

中国机械工业联合会主管  中国机械总院集团北京机电研究所有限公司 中国机械工程学会主办
联系地址:北京市海淀区学清路18号 邮编:100083
电话:+86-010-82415085 传真:+86-010-62920652
E-mail: fst@263.net(稿件) dyjsjournal@163.com(广告)
京ICP备07007000号-9