网站首页期刊简介编委会过刊目录投稿指南广告合作征订与发行联系我们English
支撑内压对某型高强钢扭力梁液压成形的影响
英文标题:Influence of supporting internal pressure on hydroforming for a certain type high-strength steel torsion beam
作者:张岩红1 许东辉2 冯海龙2 于飞3 徐斌4 赵建平5 
单位:1.石家庄财经职业学院 人居环境学院 2.石家庄市轨道交通集团有限责任公司 3.北京城建勘测设计研究院有限责任公司 4.机科发展科技股份有限公司 5.广西汽车集团有限公司 
关键词:液压成形 支撑内压 弯矩 扭力梁 壁厚分布 凹陷深度 
分类号:TG394
出版年,卷(期):页码:2021,46(6):112-116
摘要:

 通过数值模拟和实验研究了不同工艺参数对DP780高强钢扭力梁液压成形结果的影响,以改善零件的成形质量。理论证明了在V形区域内,上模与管材之间的间隙(管材凹陷深度)对液压终成形后零件的成形质量具有重要影响。因此,在预成形过程中采用内压支撑工艺,并讨论了不同支撑内压对成形结果的影响。结果表明,在预成形过程中,在适当的支撑内压范围内进行成形,可以有效地改善厚度分布。在液压终成形过程中,研究了轴向补料时支撑内压对管材成形的影响。结果表明,适当的支撑内压可以避免管端皱纹的产生,并可有效地改善管端附近的厚度分布。最后,通过液压成形工艺制造出了合格的扭力梁。

 The influences of different process parameters on hydroforming results for DP780 high-strength steel torsion beam were researched by numerical simulations and experiments to improve the forming quality of parts, and the theory proved that the clearance between upper die and tube (dent depth of tube) in the V-shaped area had an important influence on the forming quality of parts after hydroforming. Therefore, the supporting internal pressure process was used in the pre-forming process, and the influences of different supporting internal pressures on the forming results were discussed. The results show that in the pre-forming process, the forming within an appropriate supporting internal pressure range can effectively improve the thickness distribution. In the hydroforming process, the influence of supporting internal pressure on tube formability during axial feeding was analyzed. Thus, the proper supporting internal pressure can avoid wrinkles on the tube end and effectively improve the thickness distribution near the tube end. Finally, the qualified torsion beams are manufactured by hydroforming process. 

基金项目:
国家科技重大专项资助项目(2019ZX04002030)
作者简介:
张岩红(1986-),女,硕士,讲师 E-mail:sjzcjzyh@163.com
参考文献:

  


[1]Kim S H. Tool design for the tubular press forming of a rear suspension member with the finite element analysis [J]. Journal of Materials Processing Technology, 2007,192-193:181-187.


 


[2]Wang X, Li P, Wang R. Study on hydro-forming technology of manufacturing bimetallic CRA-lined pipe [J]. International Journal of Machine Tools & Manufacture, 2005, 45(4):373-378.


 


[3]Lee K T, Back H J, Lim H T, et al. Tube hydroforming process design of torsion beam type rear suspension considering durability [J]. International Journal of Modern Physics B, 2008, 22(31-32):6199-6205.


 


[4]Zhao L H, Zheng L S, Feng J Z. Failure mode analysis of torsion beam rear suspension under service conditions [J]. Engineering Failure Analysis, 2014, 36:39-48.


 


[5]Lee D, Yang C. An analytical approach for design and performance evaluation of torsion beam rear suspension [J]. Finite Elements in Analysis & Design, 2013, 63: 98-106.


 


[6]Trana K. Finite element simulation of the tube hydroforming process-bending, preforming and hydroforming [J]. Mater Process Technology, 2002, 127(3):401-408.


 


[7]Bihamta R, Bui Q H, Guillot M, et al. A new method for production of variable thickness aluminium tubes: Numerical and experimental studies [J]. Journal of Materials Processing Technology, 2011, 211(4):578-589.


 


[8]Morphy G. Tube hydroforming: Efficiency and effectiveness of pressure sequence hydroforming [J]. SAE Transpctions, 1998, 107:1297-1305.


 


[9]Ahmadi Brooghani S Y, Khalili K, Eftekhari Shahri S E, et al. Loading path optimization of a hydroformed part using multilevel response surface method [J]. The International Journal of Advanced Manufacturing Technology, 2014, 70(5-8):1523-1531.


 


[10]韩聪, 张伟玮, 谢文才, . 扭力梁内高压成形的起皱行为 [J]. 哈尔滨工业大学学报, 2013, 45(1): 85-88.


 


Han C, Zhang W W, Xie W C, et al. Analysis of wrinkling behavior of hydroformed torsion beam [J]. Journal of Harbin Institute of Technology, 2013, 45(1):85-88.


 


[11]刘伟,徐永超,陈一哲,. 薄壁曲面整体构件流体压力成形起皱机理与控制 [J]. 机械工程学报,2018, 54(9):37-44.


 


Liu W, Xu Y C, Chen Y Z, et al. Mechanism and controlling of wrinkles during hydroforming of integral thin-walled curved shell[J]. Journal of Mechanical Engineering, 2018,54(9):37-44.


 


[12]汤泽军,苑世剑,刘钢. 镁合金管材的热态内压成形起皱行为分析 [J]. 中国有色金属学报,2010, 20(3):385-389.


 


Tang Z J, Yuan S J, Liu G. Analysis of wrinkling behavior in warm hydroforming of magnesium alloy tube [J]. The Chinese Journal of Nonferrous Metals, 2010, 20(3):385-389.


 


[13]Song W J, Heo S C, Kim J, et al. Investigation on preformed shape design to improve formability in tube hydroforming process using FEM [J]. Journal of Materials Processing Technology, 2006, 177(1):658-662.


 


[14]韩聪, 贺久强, 苑世剑. 780 MPa超高强钢扭力梁内高压成形研究[J]. 精密成形工程, 2016, 8(5): 53-59.


 


Han C, He J Q, Yuan S J. Hydroforming of an automotive torsion beam with 780 MPa advanced high strength steel [J]. Journal of Netshape Forming Engineering, 2016, 8(5): 53-59.


 


[15]Yuan S J,Han CZhang W W. Optimization of pre-form shapes by response surface methodology for hydro-forming of 780 MPa torsion beam [J]. International Journal of Advanced Manufacturing Technology, 2016, 85: 1227-1237.


 


[16]Liu Z, Lang L H, Ruan S W, et al. Effect of internal pressure assisted on hydroforming for CP800 high-strength steel torsion beam[J]. Journal of the Brazilian Society of Manufacturing Sciences and Engineering, 2019,41(2):90-101.

服务与反馈:
本网站尚未开通全文下载服务】【加入收藏
《锻压技术》编辑部版权所有

中国机械工业联合会主管  中国机械总院集团北京机电研究所有限公司 中国机械工程学会主办
联系地址:北京市海淀区学清路18号 邮编:100083
电话:+86-010-82415085 传真:+86-010-62920652
E-mail: fst@263.net(稿件) dyjsjournal@163.com(广告)
京ICP备07007000号-9