Title:Investigation on hot deformation behavior of as-casted TB6 titanium alloy in β phase field
Authors: QIU Wei LU Shi-qiang OUYANG De-lai HUANG Xu LEI Li-ming 
Unit: Nanchang Hangkong University Institute of Aeronautical Materials 
KeyWords: as-casted TB6 titanium alloy  hot deformation behavior  deformation mechanism 
ClassificationCode:TG146.4
year,vol(issue):pagenumber:2010,35(6):119-123
Abstract:

Isothermal constant strain rate compression tests on the as-casted TB6 titanium alloy at temperature of 950-1100 ℃ and strain rate of  0.001-10 s-1  were conducted up to a true strain of 0.92 using the Thermecmastor-Z hot temperature simulator. The hot deformation behavior and deformation mechanisms were studied in the β phase field. The results show that characteristics of flow stress curves of this alloy mainly are of flow oscillation feature and flow softening behavior. The flow stress curve is of the small flow oscillation at 0.001~0.01 s-1 , but the wide range of flow oscillation at 10 s-1  and the flow stress curves show flow softening behavior at 0.1~1 s-1 . Microstructure observation indicates that the deformation mechanism of this alloy exhibits dynamic recrystallization feature at 0.001 s-1 , which shows dynamic recovery behavior as the main deformation mechanism at 0.01~1 s-1  and flow localization behavior at 10 s-1  , respectively. According to the effect of grain refinement and reduction of resistance of deformation, the appropriate strain rate should be no more than 0.1 s-1 .

Funds:
国家重点基础研究发展计划资助(2007CB613803);国家自然科学基金资助项目(51005112);航空科学基金资助项目(2009ZE56014)
AuthorIntro:
Reference:


[1]邵娟. 钛合金及其应用研究进展[J]. 稀有金属与硬质合金, 2007, 35(4): 61-65.
[2]曲恒磊,周廉,周义刚,等. 高强韧钛合金评述[J]. 稀有金属快报, 2004, 23(10): 5-9.
[3]王金友. 航空用钛合金[M]. 上海:科学技术出版社, 1985.
[4]Roberston D G,McShare  H B. Isothermal hot deformation behaviour of metastable β titanium alloy Ti10V2Fe3Al[J]. Materials Science and Technology,1997,13:575-583.
[5]Roberston D G,McShare H B. Analysis of high temperature flow stress of titanium alloys IMI550 and Ti10V2Fe3Al during isothermal forging[J]. Materials Science and Technology, 1998, 14(4): 339-345.
[6]Balasubrahmanyam V V,Prasad  Y V R K. Hot deformation mechanisms in metastable beta titanium alloy Ti10V2Fe3Al[J]. Materials Science and Technology, 2001, 17(4): 1222-1228.
[7]鲍如强,黄旭,黄利军,等. Ti10V2Fe3Al合金热变形的研究[J]. 材料工程, 2003,(12):3-7.
[8]Bao Ru-qiang, Huang Xu, Cao Chun-xiao. Deformation behavior and mechanisms of Ti-1023 alloy[J]. Transactions of Nonferrous Metals Society of China, 2006, (16): 274-280.
[9]Philippart I,Rack  H J. High temperature dynamic yielding in metastable Ti-6.8Mo-4.5Fe-1.5Al[J]. Materials Science and Engineering A, 1998, 243(12): 196-200.
[10]Vijayshankar M N, Ankem S. High temperature tensile deformation behavior of β-Ti alloys[J]. Materials Science and Engineering A, 1990, 129(2): 229-237.
[11]Li L X,Lou  Y,Yang  L B, et al. Flow stress behavior and deformation characteristics of Ti-3Al-5V-5Mo compressed at elevated temperatures[J]. Materials and Design, 2002, 23(5): 451-457.
[12]Seshacharyulu T,Medeiros  Steve C, Frazier William G, et al. Unstable flow during supratransus working of Ti-6Al-4V[J]. Materials Letters, 2001, 47(3): 133-139.
[13]Weiss I,Semiatin  S L. Thermomechanical processing of beta titanium alloys-an overview[J]. Materials Science and Engineering A, 1998, 243(1): 46-65.
[14]Zeng W D,Shu  Y, Zhang X M, et al. Hot workability and microstructure evolution of highly β stabilized Ti-25V-15Cr-0.3Si alloy[J]. Materials Science and Technology, 2008, 24(10): 1222-1229.
[15]Balasubrahmanyam V V,Prasad  Y V R K. Deformation behavior of beta titanium alloy Ti-10V-4.5Fe-1.5Al in hot upset forging[J]. Materials Science and Engineering A, 2002, 336(12): 150-158.
[16]陈慧琴,林好转,郭灵,等. 钛合金热变形机制及微观组织演变规律的研究进展[J]. 材料工程, 2007,  (1): 60-64.
[17]Srinivasan R, Weiss I. High temperature deformation of the near β Ti-15V-3Cr-sSn-3Al alloy[A]. Eylon D,  Boyer R R, Koss D A. Beta Titanium Alloys in the 1990s: Proceeding of a Symposium on Beta Titanium Alloys[C]. Warrendale, PA: Minerals, Metals and Materials Society, 1993.
[18]王克鲁,鲁世强,董显娟,等. Ti-6.5Al-3.5Mo-1.5Zr-0.3Si合金绝热剪切和局部流动[J]. 航空学报, 2009, 30(10) : 1967-1972.

Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com