对轿车差速器半轴锥齿轮塑性成形进行了可行性分析,采用冷摆辗方法成形齿轮锻件。利用三维有限元软件DEFORM模拟其变形过程,在变形瞬间状态及力学量场可视化环境下,得到金属流动充填规律、应力应变状况及载荷分布等。模拟结果表明,当采用阶梯状的实心毛坯,摆角1.5°,转速25.13 rad.s-1,下模进给速度5 mm.s-1时,成形效果最好。用冷摆辗方法成形高精度轿车锥齿轮锻件的方法是可行的。
|
The forming process of car differential half axle gear was analyzed and an assumption was put forward to forge the gear blank by cold rotary forging.The deformation process was also simulated with Finite Element Method software-DEFORM.Under the circumstance of instantaneous state of deformation and mechanical environment visual,the regularity of metal flow,strain-stress distribution,and rational load were obtained.The simulation results show that filling condition is ideal when rotary angle is set as 1.5°,rotate speed as 25.13 rad·s-1,feed speed as 5 mm·s1,and the blank as solid with a ladder.It is feasible to form the high precision car bevel gear by cold rotary forging.
|
基金项目:
|
河南省科技攻关项目(0424200101);;
河南科技大学基金资助项目(2004ZY050)
|
作者简介:
|
|
参考文献:
|
[1]伍太宾,任文升.汽车差速器锥齿轮的温锻制坯/冷摆辗成形加工技术研究[J].中国机械工程,2005,16(12):1106-1109.
[2]席庆坡.直齿圆柱齿轮冷精锻成形数值模拟及齿形修形研究[D].郑州:机械科学研究院,2003.4-5.
[3]陈贤杰,雷源忠,李敏贤.先进制造技术在我国的发展[A].先进制造技术发展战略学术研讨会论文集[C].上海,1998.
[4]邓克.直伞齿轮精锻技术的应用及发展[J].安徽工业大学学报,2005,22(2):169-173.
[5]张宗仁,顾良,刘纯亮.浅谈精密模锻成形工艺[J].金属成形工艺,1998,16(3):20-22.
[6]林和荣,王幼华.摆动辗压成形过程有限元模拟[J].江西有色金属,2005,9(3):40-42.
[7]敖学安.SC110型汽车半轴齿轮的冷摆辗成形[J].金属成形工艺,1998,16(5):19-22.
|
服务与反馈:
|
【文章下载】【加入收藏】
|
|
|