摘要:
|
针对不锈钢板拉深时产生缺陷的原因进行分析,提出了解决措施,并提出了减少汽车消声器壳成形缺陷的对策,取得了较好的效果。
|
The reasons of defects in stainless steel sheet deep-drawing are analyzed and the settling measures are offered.The countermeasure to reduce the forming defects of automobile muffler is also given here and we have obtained better result than that before.
|