内压对小直径薄壁U型波纹管成形规律的影响
英文标题:Effect of internal pressure on forming law of thin-wall U-shaped bellows with small diamete
作者:李凯 苗晓军 皇涛 蒋宇宁 赵家鑫 
单位:平高集团有限公司 河南科技大 有色金属共性技术河南省协同创新中心 
关键词:波纹管 内压 成形规律 壁厚减薄率 数值模拟 
分类号:TG376
出版年,卷(期):页码:2020,45(10):66-72
摘要:

 为了研究内压对小直径薄壁U型波纹管的壁厚减薄率的影响行为,采用数值模拟分析的方法,基于ANSYS/LS-DYNA有限元分析软件,建立了小直径薄壁U型316L奥氏体不锈钢波纹管的内压成形过程的有限元模型,获得了小直径薄壁U型波纹管内压成形过程中的等效应力、等效应变和壁厚减薄率的分布演变规律。在相同的轴向进给位移条件下,获得了不同的内压对小直径薄壁U型波纹管的壁厚减薄率分布的影响规律,获得了成形质量合格的小直径薄壁U型波纹管的成形内压范围,研究结果为小直径薄壁U型波纹管的内压成形工艺的设计提供了数据参考。

 In order to study the effect behavior of internal pressure on the wall thickness thinning rate of thin-wall U-shaped bellows with small diameter, using the numerical simulation analysis method, the finite element model of internal pressure forming process for the thin-wall U-shaped 316L austenitic stainless steel bellows with small diameter was established based on ANSYS/LS-DYNA finite element analysis software. The distributions and evolution laws of equivalent stress, equivalent strain and wall thickness thinning rate during the internal pressure forming process of thin-wall U-shaped bellows with small diameter were obtained. The effect law of different pressures on the wall distribution of thickness thinning rate for thin-wall U-shaped bellows with small diameter under the same axial feeding displacement conditions was obtained. The forming internal pressure range of qualified forming thin-wall U-shaped bellows with small diameter was obtained. The research results provide the data reference to the design of internal pressure forming process for thin-wall U-shaped bellows with small diameter.

基金项目:
国家自然科学基金资助项目(51875176);国家电网有限公司总部科技资助项目(B491 BG190013)
作者简介:
李凯(1984-),男,硕士,高级工程师 E-mail:007zzulikai@163.com 通讯作者:皇涛(1983-),男,博士,副教授 E-mail:huangtao@haust.edu.cn
参考文献:

 
[1]唐治东.波纹管液压成形过程的数值模拟与实验研究
[D].杭州:浙江工业大学, 2015.


Tang Z D. Numerical Simulation and Experimental Study of Hydroforming Process of Bellows
[D]. Hangzhou: Zhejiang University of Technology, 2015. 


[2]Abrantes J P, Szabo-Ponce A, CtF Batalha. Experimental and numerical simulation of tube hydroforming
[J]. Journal of Materials Processing Technology, 2005, 164(15): 1140-1147.


[3]李艳艳.V形膨胀节的承载和补偿能力分析及膨胀节成形过程的模拟
[D].北京:北京化工大学,2009.

Li Y Y. V-shaped Expansion Joint Load-bearing and Compensation Capacity Analysis and Expansion Joint Forming Process Simulation
[D]. Beijing: Beijing University of Chemical Technology, 2009.



[4]Yuan S, Yuan W, Wang X. Effect of wrinkling behavior on formability and thickness distribution in tube hydroforming
[J]. Journal of Materials Processing Technology, 2006, 177(1-3):668-671.


[5]王小松,苑世剑,王仲仁.内高压成形起皱行为的研究
[J].金属学报,2003, 39(12): 1276-1280.

Wang X S, Yuan S J, Wang Z R. Research on wrinkling behavior of internal high pressure forming
[J]. Acta Metallurgica Sinica, 2003, 39(12): 1276-1280.


[6]汤泽军,何祝斌,苑世剑.内高压成形过程塑形失稳起皱分析
[J].机械工程学报,2008, 44(5): 34-38. 

Tang Z J, He Z B, Yuan S J. Analysis of wrinkling during instability during internal high pressure forming
[J]. Journal of Mechanical Engineering, 2008, 44(5): 34-38.


[7]苑文婧,刘晓航,田浩彬.双锥形管液压成形过程中破裂和起皱的力学条件
[J].上海第二工业大学学报, 2012, 29(1): 12-19.

Yuan W J, Liu X H, Tian H B. The mechanical conditions of rupture and wrinkling during the hydroforming of the double-cone tube
[J]. Journal of Shanghai Second Polytechnic University, 2012, 29(1): 12-19.


[8]郭煜敬,王志刚,金光耀,等. 液压成形波纹管减薄率的数值模拟研究
[J].浙江工业大学学报,2019,47(1):58-62.

Guo Y J, Wang Z G, Jin G Y, et al. Numerical simulation of the thinning rate of hydroformed bellows
[J]. Journal of Zhejiang University of Technology, 2019, 47(1): 58-62.


[9]Fang K J, Hsiao P Y. Optimization of loading conditions for tube hydroforming
[J]. Journal of Materials Processing Technology, 2003, 140: 520-524.


[10]Yang J B,Jeon B H,Oh S I. Design sensitivity analysis and optimization of the hydroforming process
[J]. Journal of Materials Processing Technology,2001,113(1/2/3):666-672.


[11]崔磊,刘静,李兰云. 基于响应面法的双层316L/Inconel625波纹管液压胀形工艺参数优化
[J].兵器材料科学与工程,2018,41(6):19-26.

Cui L, Liu J, Li L Y. Optimization of hydraulic bulging process parameters of double-layer 316L/Inconel625 bellows based on response surface method
[J]. Ordnance Material Science and Engineering, 2018, 41(6):19-26.


[12]陈杰.管材内高压成形数值模拟与工艺研究
[D].上海:上海交通大学,2013.

Chen J. Numerical Simulation and Process Study of High Pressure Forming in Pipes
[D]. Shanghai: Shanghai Jiao Tong University, 2013.


[13]唐治东.波纹管液压成形过程的数值模拟与实验研究
[D].杭州:浙江工业大学,2015.

Tang Z D. Numerical Simulation and Experimental Research on the Process of Bellows Hydroforming
[D].Hangzhou:Zhejiang University of Technology, 2015.

服务与反馈:
本网站尚未开通全文下载服务】【加入收藏
《锻压技术》编辑部版权所有

中国机械工业联合会主管  中国机械总院集团北京机电研究所有限公司 中国机械工程学会主办
联系地址:北京市海淀区学清路18号 邮编:100083
电话:+86-010-82415085 传真:+86-010-62920652
E-mail: fst@263.net(稿件) dyjsjournal@163.com(广告)
京ICP备07007000号-9