[1]刘以波.TA2工业纯钛高温组织演变研究[D].上海:上海交通大学,2010.
Liu Y B. Microstructure Evolution of TA2 Commercial Pure Titanium at High Temperature [D]. Shanghai:Shanghai Jiao Tong University, 2010.
[2]李彤,苏松林,安邦,等.高性能低成本钛合金生产应用现状[J].特钢技术,2024,30(3):8-11,15.
Li T,Su S L,An B,et al. Current status of production and application of high-performance and low-cost titanium alloys[J]. Special Steel Technology,2024,30(3):8-11,15.
[3]尚筱迪.工业纯钛TA2热压缩变形行为及微观组织演变[D].西安:西安建筑科技大学,2019.
Shang X D. Hot Deformation Behavior and Microstructure Evolution of TA2 [D]. Xi′an: Xi′an University of Architecture and Technology, 2019.
[4]王怀柳.浅析工艺参数对TA2挤压管材质量的影响[J].特钢技术,2016,22(2):12-17.
Wang H L. Influence of process parameters on the quality of TA2 extruded pipe [J]. Special Steel Technology, 2016,22 (2): 12-17.
[5]郭玲,谢翀博.纯钛管坯热挤压工艺改进[J].机械制造,2015,53(6):71-73.
Guo L, Xie C B. Improvement of hot extrusion process for pure titanium tube billets [J]. Machinery, 2015,53 (6): 71-73.
[6]杨英丽,卢亚锋,郭荻子,等.氧含量及轧制工艺对纯钛管材性能的影响[J].钛工业进展,2011,28(5):27-30.
Yang Y L, Lu Y F, Guo D Z, et al. Effect of oxygen content on properties of commercial pure titanium tubes [J]. Titanium Industry Progress, 2011, 28 (5): 27-30.
[7]贠鹏飞,杨英丽,郭荻子,等.轧制Q值对小口径TA2管材组织和性能的影响[J].钛工业进展,2012,29(2):24-27.
Yun P F, Yang Y L, Guo D Z, et al. Effect of cold-rolling Q on microstructure and mechanical property of small-caliber TA2 tube [J]. Titanium Industry Progress, 2012,29 (2): 24-27.
[8]Pumpyanskiy D A, Illarionov A G,Vodolazskiy F, et al.Material science aspects of titanium tube production. Part 2: Production of cold-rolled tubes[J].Metallurgist,2024,67(9-10):1482-1493.
[9]李永林,王璐,孟鑫,等.两辊冷轧纯钛管材的工艺研究[J].热加工工艺,2019,48(17):42-45.
Li Y L, Wang L, Meng X, et al. Study on technology of cold rolling pure titanium tube with two rolls [J]. Hot Working Technology, 2019,48 (17): 42-45.
[10]Xing J, Chen H,Yang Y L,et al. Effect of drawing processing on mechanical properties and textures of TA2 pipes[J].Rare Metal Materials and Engineering, 2015,44 (2): 485-488.
[11]马浩. 纯钛及钛合金强力旋压损伤演化规律及韧性断裂预测[D]. 哈尔滨:哈尔滨工业大学,2017.
Ma H. Damage Evolution and Ductile Fracture Prediction in Power Spinning of Pure Titanium and Titanium Alloys [D]. Harbin:Harbin Institute of Technology, 2017. [12]Li C, Shuang Y H, Chen J X, et al.Research on the impact of mandrels in titanium tubes during tube continuous rolling[J].Materials Research Express,2023,10(8):086512. [13]雷亮.连轧无缝钢管轧制力计算模型研究[D]. 长沙:中南大学,2004. Lei L. Research on Rolling Force Calculation Model for Continuous Rolling of Seamless Steel Tube [D]. Changsha:Central South University, 2004. [14]肖成.无缝钢管连轧过程建模与轧制规程优化[D].长沙:中南大学,2014. Xiao C. Modeling and Rolling Schedule Optimization of Seamless Steel Tube Rolling Process [D].Changsha: Central South University, 2014. [15]周研.小直径无缝钢管短流程连轧特征与关键技术研究[D].太原:太原科技大学,2016. Zhou Y. Key Technology and Characteristics Study of the Continual Mandrel Rolling Compact Process for Producing Minor Diameter Seamless Steel Tubes [D]. Taiyuan:Taiyuan University of Science and Technology, 2016. [16]汤涛,邹树梁.无缝钢管连轧过程数值模拟及参数优化[J].钢铁研究学报,2012,24(11):6-10. Tang T, Zou S L. Numerical simulation and parameter optimization for tandem rolling process of seamless steel tube [J]. Journal of Iron and Steel Research, 2012,24 (11): 6-10. [17]赵志毅,董凯,余勇,等.全浮动芯棒连轧管机组轧制力测试与研究[J].钢管,2006(4):1-5. Zhao Z Y, Dong K, Yu Y, et al. Measurement of and study on rolling forces of full-floating mandrel mill [J]. Steel Pipe, 2006(4): 1-5. [18]代佳,双远华,苟毓俊,等.压下率对AZ31B镁合金管材纵连轧力能参数的影响[J].热加工工艺,2020,49(11):86-89. Dai J, Shuang Y H, Gou Y J, et al. Effect of reduction rate on force-energy parameters of AZ31B magnesium alloy tube during continual mandrel rolling process [J]. Hot Working Technology, 2020,49 (11): 86-89. [19]代佳.镁合金管材纵连轧工艺及实验研究[D].太原:太原科技大学,2020. Dai J. Experimental Study on Longitudinal Continuous Rolling Technology of Magnesium Alloy Pipe [D]. Taiyuan:Taiyuan University of Science and Technology, 2020.
|