Abstract:
|
The stamping formability of non uniform thick tailor welded blanks(TWBs)is quite affected by the weld seams and its orientation as well as the ratio between the thin sheet and the thick sheet.In this paper,effects of welding techniques on the formability of TWBs,such as laser welding,seam welding and TIG welding,are discussed.Deep drawing of semi spherical shells and square cups is carried out,the non uniform deformation behaviors and the movement of the weld seams are summarized.
|
Funds:
|
|
AuthorIntro:
|
|
Reference:
|
1 FSaunders,RHWagoner.Formingoftailor weldedblanks.Metallur gicalandMaterialsTransactionsA ,1996,27(9):2605~2616
2 PJBolt,WBBavel,AAJunaiImprovingtheformabilityoftailor madeblanksbyusingacounterforceProceedingsofthe5thInterna tionalConferenceSheMet’97,UniversityofUlster,NorthenIreland,1997:463~469
3 AWinterEnvironmentallyfriendlymanufacturingoftailor madeblanksProceedingsofthe20thBiennialCongress,IDDRG’98,Brus sels,Belgium:191~202
4 张士宏,程欣,朗利辉,徐福昌拼焊板焊接工艺及其对拼焊板塑性变形影响的试验研究材料科学与工艺,1999,增刊,Vol7:143~147
5 BKinsey,JCaoAnovelformingtechnologyfortailor weldedblanksJournalofMaterialsProcessingTechnology,2000,99(1):145~153
|