Title:New technology of solid granule medium deep drawing and forming die design
Authors: ZHANG Ling-yun YUAN Hai-huan(Liaoning Key Lab of Digital Processes Simulation and Test Technology Shenyang Institute of Aeronautical Engineering Shenyang 110136 China) 
Unit:  
KeyWords: solid granules deep drawing die design 
ClassificationCode:TG386.41
year,vol(issue):pagenumber:2010,35(1):93-95
Abstract:
Considering the difficult seal of liquid media and complex installation etc.existing in the traditional hydro-mechanical deep drawing,a new process was proposed,which replaced the original liquid medium with the solid granules to solve these problems.Force analysis in the drawing process reveals that the new technology of solid granulemedium deep drawing can effectively reduce tensile stress in the forming process,and it is helpful to improve material formability.Through the experiment of the LY12M sheet with the self-designed die set,the feasibility of the solid granule medium deep drawing process was verified.The limited deep drawing coefficient can be up to 0.51,superior to the traditional rigidity-die deep drawing process.
Funds:
AuthorIntro:
Reference:
[1]郎利辉.板材液压成形及无模充液拉深技术[J].塑性工程学报,2002,12(4):30-32.
[2]赵军.圆锥形件拉深成形智能化的研究[D].哈尔滨:哈尔滨工业大学,1997.
[3]欧阳仁.液压机械拉深工艺的研究[J].锻压技术,1980,5(1):11-20.
[4]刑晓东,郭斌,罗荣华.材料粘性压力成形技术研究[J].中国机械工程,2001,12(2):231-234.
[5]赵长财,王银思.固体颗粒介质成形工艺几何参数研究[J].塑性工程学报,2008,10(5):116-120.
[6]赵长财,王银思,李晓丹,等.固体颗粒介质的传压性能实验研究[J].塑性工程学报,2006,13(2):85-88.
[7]Lawrenz K J.在液压深拉深时板料拉裂极限的求法[J].张德荣,译.锻压技术,1981,6(6):15-18.
[8]李新均,万敏,周贤宾.粘性介质成形工艺特点与应用分析[J].锻压技术,1999,24(6):28-30.
[9]王冀.筒形件充液拉深的理论研究和数值模拟及计算机控制[D].西安:西安交通大学,2002.
[10]肖景容.冲压工艺学[M].北京:科学出版社,1988.
[11]陈明祥.弹塑性力学[M].北京:机械工业出版社,2007.
[12]王孝培.冲压手册[M].北京:机械工业出版社,1986.
Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com