Abstract:
|
According to the properties requirement of cold rollers, materials of Cr5 with high hardenability, high stability after tempering are chosen and measures of two-steps refinement, high forging ratio and special heat treatment are taken to get the final rollers with high purity and homogeneous structure to meet the requirement of anti-fatigue and anti-accidence.
|