Title:Deformation behavior of non-metallic inclusions of FGH96 alloy in extrusion process
Authors: ZHANG Min-cong  FANG Shuang  CHEN You-hong  SUN Xing  DONG Yun-peng  WANG Shu-yun 
Unit: Beijing Institute of Aeronautical Materials 
KeyWords: FGH96 alloy  non-metallic inclusion  hot extrusion  deformation behaviors 
ClassificationCode:TG132.32
year,vol(issue):pagenumber:2013,38(6):132-137
Abstract:

The morphology and deformationcharac terisitics of non-metallic inclusions Al2O3 and SiO2 in the hot isostatic pressing process and the high-temperature extrusion process were analyzed by the hot extrusion deformation test of FGH96 alloy in the state of high-temperature isostatic pressing. The results show that Al2O3 has no reaction in FGH96 alloy and the transition zone between Al2O3 and FGH96 alloy is mechanical combination during the plastic deformation, whereas SiO2 reacts with aluminum and titanium in the environment of high temperature and high pressure. The reaction zone is formed in the interface between SiO2 and FGH96 alloy. In the extrusion process, the FGH96 alloy is situated in strong tri-axial pressure. The non-metallic inclusions are pulled into a discontinuous line in extrusion direction and areas of inclusions are constricted in the perpendicular of extrusion direction. In summary, the large extrusion ratio can break the non-metallic inclusions in FGH96 alloy effectively,refine the grain and improve the purity of FGH96 alloy plate.
 

Funds:
AuthorIntro:
Reference:


[1]Infante V, Silva J M, Freitas M, et al. Failures analysis of compressor blades of aeroengines due to service[J]. Engineering Failure Analysis, 2009,16:1118-1125.
[2]李园春, 王淑云. 国内粉末高温合金涡轮盘件制造技术的发展现状[J]. 稀有金属, 2001, 25(3): 226-229.Li Y C, Wang S Y. Development on manufacture of turbine disk from superalloy powder in China[J]. Chinese Journal of Rare Metals, 2001, 25(3): 226-229.
[3]李惠曲, 王淑云, 东赟鹏, 等. 粉末高温合金等温锻造过程非金属夹杂物的变形特征[J]. 新技术新工艺, 2009, (5): 93-95.Li H Q, Wang S Y, Dong Y P, et al. Deformation character of non-metallic inclusions in powder superalloy during isothermal casting[J]. New Technology New Process, 2009, (5): 93-95.
[4]王旭青. FGH96高温合金粉末显微组织及夹杂分析[J]. 粉末冶金技术, 2001, 19(2): 1-4.Wang X Q. The analysis of microstructure and inclusion of FGH96-powder of 750℃ superalloy[J]. Powder Metallurgy Technology, 2001, 19(2): 1-4.
[5]Huron E S, Roth P G. The influences on low cycle fatigue life in a P/M nickel-base disk superalloy[A]. Proceedings of the Eight International Symposium on Superalloy
[C]. Warrendale: The Minerals, Metals & Materials Society, 1996.
[6]国为民, 吴剑涛, 张凤戈, 等. 粉末高温合金中夹杂物特性及与不同成型工艺的关系[J]. 材料导报, 2004, 18(11): 87-91.Guo W M, Wu J T, Zhang F G, et al. Characteristic of inclusions and its relationship with different forming processes in powder superalloy[J]. Materials Review, 2004, 18(11):87-91.
[7]邹金文, 汪武祥. 粉末高温合金中夹杂物特性及其质量控制[J]. 粉末冶金技术, 2001, 19(1): 87-91.Zou J W, Wang W X. Characteristic and quality control of inclusions in P/M superalloy[J]. Powder Metallurgy Technology, 2001, 19(1):87-91.
[8]Barrie R L, Gabb T P, Telesman J, et al. Effectiveness of shot peening in suppressing fatigue cracking at non-metallic inclusions in Udimet 720[J]. Materials Science and Engineering A, 2008, 474(1): 71-81.
[9]Gabb T P, Telesman J, Kantzos P T, et al. Initial assessment of the effects of nonmetallic inclusions on fatigue life of powder-metallurgy-processed Udimet 720[R]. NASA/TM-2002-211571, Washington: National Aeronautics and Space Administration, 2002.
[10]Shenoy M M, Kumar R S, Mcdowell D L. Modeling effects of non-metallic inclusions on LCF in DS nickel-base superalloys[J]. International Journal of Fatigue, 2005,27(2):113-127.
[11]Chang M, Koul A K, Cooper C. Damage tolerance of P/M turbine disc materials[A]. Proceedings of the Eight International Symposium on Superalloy
[C]. Warrendale: The Minerals, Metals & Materials Society, 1996.
[12]王淑云,张敏聪,东赟鹏, 等. FGH96合金热挤压棒材超塑性研究[J]. 材料工程, 2012,384(7):24-28.Wang S Y, Zhang M C, Dong Y P, et al. Study on superplasticity of extruded FGH96 Alloy[J]. Journal of Materials Engineering, 2012, 384(7):24-28.
[13]刘趁意,王淑云,李付国, 等. 粉末高温合金挤压变形组织及变形机理研究[J]. 锻压装备与制造技术, 2009, 44(1):84-87.Liu C Y, Wang S Y, Li F G, et al. The procedure and mechanics research of extrusion deformation for FGH96 alloy[J]. China Metalforming Equipment Manufacturing Technology, 2009, 44(1):84-87.
[14]Zhang M C, Liu C Y, Wang S Y. Deformation behaviors of non-metallic inclusion in FGH96 superalloy during different plastic processes[J]. Advanced Materials Research, 2012, 538-541:1187-1191.
[15]刘趁意,王淑云,东赟鹏, 等. FGH96合金挤压过程的数值模拟与试验研究[J]. 锻压装备与制造技术, 2010, 45(2):103-107.Liu C Y, Wang S Y, Dong Y P, et al. Numerical simulation and testing study on extrusion process of FGH96 alloy[J]. China Metalforming Equipment Manufacturing Technology, 2010, 45(2):103-107.

Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com