Title:Investigation on interface reaction in continuous SiC fiber reinforced titanium composites
Authors: Li Hu  Huang Xu Huang Hao  Wang Minjuan Xie Chuan 
Unit: Beijing Institute of Aeronautical Materials 
KeyWords: titanium composites SiC fiber interface reaction 
ClassificationCode:
year,vol(issue):pagenumber:2016,41(4):103-108
Abstract:

It was studied the interface reaction rate and product in continuous SiC fiber reinforced Titanium composite. The continuous W core SiC fiber reinforced Ti17 composite was fabricated by HIP technology through matrix-fiber coated method, and then the composite was exposed to various temperatures and time. The thickness of the interface reaction layer, the chemical component and the reaction product of the interface were observed and analyzed by Scanning Electron Microscopy(SEM), Transmission Electron Microscopy(TEM) and Energy Design Suite(EDS). The results demonstrate that the carbon coating can protect the SiC fiber efficiently, and the main elements in the interface reaction layer are Ti and C. Furthermore, the interface reaction product of as-processed sample is TiC1-x , which has a fine grain size near the carbon coating and coarse grain size near the matrix. Thus, the interface reaction and its layer thickness increase after thermal exposure, the growth of the interface layer obeys parabola law, and the kinetic parameters are frequency factor k0=1.33×10-3 m·s-1/2 and activation energy Q=243.22 kJ·mol-1, respectively.

Funds:
科技部国家重点基础研究发展计划资助项目(2007CB613803)
AuthorIntro:
李虎(1989-),男,硕士研究生
Reference:

[1]杨锐,石南林,王玉敏,等. SiC纤维增强钛基复合材料研究进展[J] .钛工业进展,2005,22(5):32-36.

Yang R, Shi N L, Wang Y M, et al. Recent progress in SiC fibre reinforced titanium matrix composites [J]. Titanium Industry Process, 2005,22(5):32-36.

[2]Clyne T W, Withers P J. An Introduction to Metal Matrix Composites[M].New York:Cambridge University Press,1993.

[3]Xun Y W, Tan M J, Zhou J T. Processing and interface stability of SiC fiber reinforced Ti-15V-3Cr matrix composites [J]. Journal of Material Processing Technology, 2000,102(s1-3):215-220.

[4]Debolt H, Krukonis V K. Improvement of manufacturing methods for the production of low cost silicon carbide filament[P].US:Air Force Contract F33615-72-C-1177, Report No. AFML-TR-73-140, 1973.

[5]Zhang W, Yang Y Q,Zhao G M, et al. Interfacial reaction studies of B4C coated and C-coated SiC fiber reinforced Ti-43Al-9V composites [J]. Intermetallics, 2014 ,50(1):14-19.

[6]Fan Z,Guo Z X,Cantor B. The kinetics and mechanism of interfacial reaction in sigma fibre-reinforced Ti MMCs [J]. Composites Part A, 1997 ,28(2):131-140.

[7]Thomas D McGarry,Marek-Jerzy P,Franklin E Wawner. Evaluation of reaction barrier compensating coating on SCS-6 fibers in Ti-24al-11Nb (at%) composites [J]. Composites Engineering, 1995, 5 (7): 951-974.

[8]杨延清,刘玉成,马志军,等. SiCf/Ti-6Al-4V复合材料界面反应动力学[J]. 稀有金属快报, 2006, 25(12):18-21.

Yang Y Q, Liu Y C, Ma Z J,et al. Kinetics of interfacial reaction in SiCf/Ti- 6Al- 4V composites [J]. Rare Metals Letters, 2006, 25(12): 18-21.

[9]赵永庆,周廉,Alain Vassel,等. SiC长纤维增强钛合金基复合材料的界面研究[J]. 稀有金属材料与工程,2004, 33(4):359-362.

Zhao Y Q, Zhou L, Alain Vassel, et al. Study of interfaces in titanium alloy composites reinforced with continuous SiC fibers [J]. Rare Metal Materials and Engineering, 2004, 33(4):359-362.

[10]Yang Y Q, Werne r A, Dudek H J,et al. TEM investigations of interfacial processes in SCS-6 SiC/TiB2/Super α2 composites [J]. Composites: Part A, 1999,30(1):1209-1214.

[11]朱艳,杨延清,马志军,等. SiC/Ti基复合材料界面反应的热力学研究[J].稀有金属材料与工程,2002, 31(4):279-282.

Zhu Yan, Yang Y Q,Ma Z J, et al. Thermodynamic studies on interfacial reactions in SiC-fiber-reinforced Ti-martrix composites [J]. Rare Metal Materials and Engineering, 2002, 31(4):279-282.

[12]Guo S Q, Kagawa Y, Saito H,et al.Microstructural characterization of interface in SiC fiber-reinforced Ti-15V-3Cr-3Al-3Sn matrix composite[J]. Materials Science and Engineering: A, 1998,246(s1-2):25-35.

[13]Ruhle M, Evans A G, Hirth J P,et al. Metal-Ceramic Interfaces [M]. Oxford:Pergamon Press,1990.

[14]王玉敏.连续SiC(f)/Ti-6Al-4V复合材料的制备、界面反应及拉伸性能研究[D].沈阳:中国科学院金属研究所,2005.

Wang Y M. Study on Fabrication, Interface Reaction and Tensile Strength of Continous SiC(f)/Ti-6Al-4VComposites [D]. Shenyang:Institute of Metal Research, Chinese Academy of Sciences, 2005.

Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com