Title:Influence of supporting internal pressure on hydroforming for a certain type high-strength steel torsion beam
Authors:  
Unit:  
KeyWords: hydroforming  supporting internal internal pressure  bending moment  torsion beam  thickness distribution  dent depth 
ClassificationCode:TG394
year,vol(issue):pagenumber:2021,46(6):112-116
Abstract:

 The influences of different process parameters on hydroforming results for DP780 high-strength steel torsion beam were researched by numerical simulations and experiments to improve the forming quality of parts, and the theory proved that the clearance between upper die and tube (dent depth of tube) in the V-shaped area had an important influence on the forming quality of parts after hydroforming. Therefore, the supporting internal pressure process was used in the pre-forming process, and the influences of different supporting internal pressures on the forming results were discussed. The results show that in the pre-forming process, the forming within an appropriate supporting internal pressure range can effectively improve the thickness distribution. In the hydroforming process, the influence of supporting internal pressure on tube formability during axial feeding was analyzed. Thus, the proper supporting internal pressure can avoid wrinkles on the tube end and effectively improve the thickness distribution near the tube end. Finally, the qualified torsion beams are manufactured by hydroforming process. 

Funds:
国家科技重大专项资助项目(2019ZX04002030)
AuthorIntro:
张岩红(1986-),女,硕士,讲师 E-mail:sjzcjzyh@163.com
Reference:

  


[1]Kim S H. Tool design for the tubular press forming of a rear suspension member with the finite element analysis [J]. Journal of Materials Processing Technology, 2007,192-193:181-187.


 


[2]Wang X, Li P, Wang R. Study on hydro-forming technology of manufacturing bimetallic CRA-lined pipe [J]. International Journal of Machine Tools & Manufacture, 2005, 45(4):373-378.


 


[3]Lee K T, Back H J, Lim H T, et al. Tube hydroforming process design of torsion beam type rear suspension considering durability [J]. International Journal of Modern Physics B, 2008, 22(31-32):6199-6205.


 


[4]Zhao L H, Zheng L S, Feng J Z. Failure mode analysis of torsion beam rear suspension under service conditions [J]. Engineering Failure Analysis, 2014, 36:39-48.


 


[5]Lee D, Yang C. An analytical approach for design and performance evaluation of torsion beam rear suspension [J]. Finite Elements in Analysis & Design, 2013, 63: 98-106.


 


[6]Trana K. Finite element simulation of the tube hydroforming process-bending, preforming and hydroforming [J]. Mater Process Technology, 2002, 127(3):401-408.


 


[7]Bihamta R, Bui Q H, Guillot M, et al. A new method for production of variable thickness aluminium tubes: Numerical and experimental studies [J]. Journal of Materials Processing Technology, 2011, 211(4):578-589.


 


[8]Morphy G. Tube hydroforming: Efficiency and effectiveness of pressure sequence hydroforming [J]. SAE Transpctions, 1998, 107:1297-1305.


 


[9]Ahmadi Brooghani S Y, Khalili K, Eftekhari Shahri S E, et al. Loading path optimization of a hydroformed part using multilevel response surface method [J]. The International Journal of Advanced Manufacturing Technology, 2014, 70(5-8):1523-1531.


 


[10]韩聪, 张伟玮, 谢文才, . 扭力梁内高压成形的起皱行为 [J]. 哈尔滨工业大学学报, 2013, 45(1): 85-88.


 


Han C, Zhang W W, Xie W C, et al. Analysis of wrinkling behavior of hydroformed torsion beam [J]. Journal of Harbin Institute of Technology, 2013, 45(1):85-88.


 


[11]刘伟,徐永超,陈一哲,. 薄壁曲面整体构件流体压力成形起皱机理与控制 [J]. 机械工程学报,2018, 54(9):37-44.


 


Liu W, Xu Y C, Chen Y Z, et al. Mechanism and controlling of wrinkles during hydroforming of integral thin-walled curved shell[J]. Journal of Mechanical Engineering, 2018,54(9):37-44.


 


[12]汤泽军,苑世剑,刘钢. 镁合金管材的热态内压成形起皱行为分析 [J]. 中国有色金属学报,2010, 20(3):385-389.


 


Tang Z J, Yuan S J, Liu G. Analysis of wrinkling behavior in warm hydroforming of magnesium alloy tube [J]. The Chinese Journal of Nonferrous Metals, 2010, 20(3):385-389.


 


[13]Song W J, Heo S C, Kim J, et al. Investigation on preformed shape design to improve formability in tube hydroforming process using FEM [J]. Journal of Materials Processing Technology, 2006, 177(1):658-662.


 


[14]韩聪, 贺久强, 苑世剑. 780 MPa超高强钢扭力梁内高压成形研究[J]. 精密成形工程, 2016, 8(5): 53-59.


 


Han C, He J Q, Yuan S J. Hydroforming of an automotive torsion beam with 780 MPa advanced high strength steel [J]. Journal of Netshape Forming Engineering, 2016, 8(5): 53-59.


 


[15]Yuan S J,Han CZhang W W. Optimization of pre-form shapes by response surface methodology for hydro-forming of 780 MPa torsion beam [J]. International Journal of Advanced Manufacturing Technology, 2016, 85: 1227-1237.


 


[16]Liu Z, Lang L H, Ruan S W, et al. Effect of internal pressure assisted on hydroforming for CP800 high-strength steel torsion beam[J]. Journal of the Brazilian Society of Manufacturing Sciences and Engineering, 2019,41(2):90-101.

Service:
This site has not yet opened Download Service】【Add Favorite
Copyright Forging & Stamping Technology.All rights reserved
 Sponsored by: Beijing Research Institute of Mechanical and Electrical Technology; Society for Technology of Plasticity, CMES
Tel: +86-010-62920652 +86-010-82415085     Fax:+86-010-62920652
Address: No.18 Xueqing Road, Beijing 100083, P. R. China
 E-mail: fst@263.net    dyjsgg@163.com